| Fin/Absorber Structure & Item
 | Fusion Bonding Type | Package Ultrasonic Welding Type | Laser Welding Type | Normal Ultrasonic Welding Type | 
 
            
            | Photos |    |    |    |     | 
 
            
            | Base Material With Coating | Anodic Oxidation : Fusion Bonding Alumnium Strip
 +  Copper Tube (riser)
 | Anodic Oxidation : Alumnium Strip +  "U"shape
 Aluminum Strip +  Copper Tube (riser)
 | Blue Selective : Full Copper Plate +
 Copper Tube (riser)
 | Anodic Oxidation: Aluminum Strip +
 Copper Tube (riser)
 | 
 
            
            | Black Chrome / Blue Selective : Full Aluminum Plate
 + "U"shape Aluminum Strip
 +  Copper Tube (riser)
 | Black Chrome : Copper Strip+
 Copper Tube (riser)
 | 
 
            
            | Structure | Fusion Bonding for two pieces of Alumnium Strip and  Alumnium  tube ,
 then blowing up Alumium tube.
 | Using "U"shape Aluminum Strip to pack Copper Tube (riser)  ,
 then Ultrasonic Welding "U"shape
 Aluminum Strip and Strip/Plate.
 | Laser Welding between Full Copper Plate and
 Copper Tube (riser) directly
 | Normal Ultrasonic welding between Strip and  Copper Tube (riser)  directly
 | 
 
            
            | Structure Stability | Insert Riser Tube inside fusion bonding Strip and pressure tightly ,
 More stronger for the structure.
 | Same material welding together , more stronger for the structure.
 | Normal , Only the welding points between Strip and Copper Tube (riser) .
 | Normal .Only about 2-3mm welding line between Strip and  Copper Tube (riser) .
 A little damage for the fin surface .
 | 
 
            
            | Conductive Surface | 360° Heat Exchange | 360° Heat Exchange | Only welding points for heat exchange . | Only 3-4mm width welding line for heat exchange .
 | 
 
            
            | Thermal Efficiency | Higher | High | Normal | Normal |